PWHT of 410 to 316 Stainless steel
Sep 30, 2019· Lets just call out a 410 with a carbon content of 5% with a thickness of .550".750". the PWHT should be 600F When i have met all the requirements and let it cool while wrapped in an asbestos blanket and black light the weld, there appears to be a crack as if the weld did not melt the the stainless to the fill rod.